偏析干预下体心立方金属再结晶织构竞争 |
| 常松涛, 张芳, 沙玉辉, 左良 |
|
Recrystallization Texture Competition Mediated by Segregation Element in Body-Centered Cubic Metals |
| CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang |
| 图4 无Sb和含Sb的Fe-3%Si冷轧板EBSD取向成像图和几何必需位错(GND)密度成像图 |
| Fig.4 EBSD orientation image maps (a, c) and GND density maps (b, d) in cold rolled Fe-3%Si sheets without (a, b) and with (c, d) Sb addition (GND—geometrically necessary dislocation, ND—normal direction, RD—rolling direction) |
|