偏析干预下体心立方金属再结晶织构竞争 |
| 常松涛, 张芳, 沙玉辉, 左良 |
|
Recrystallization Texture Competition Mediated by Segregation Element in Body-Centered Cubic Metals |
| CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang |
| 图2 无Sb和含Sb的Fe-3%Si再结晶板亚表层和中心层ODF的φ2 = 0°和45°截面图 |
| Fig.2 Constant φ2 = 0° and 45° sections of ODFs at subsurface and center layers in recrystallized Fe-3%Si sheets without (a) and with (b) Sb addition |
|