FeMnCoCrNi高熵合金双晶微柱变形机制的分子动力学模拟 |
| 张海峰, 闫海乐, 方烽, 贾楠 |
|
Molecular Dynamic Simulations of Deformation Mechanisms for FeMnCoCrNi High-Entropy Alloy Bicrystal Micropillars |
| ZHANG Haifeng, YAN Haile, FANG Feng, JIA Nan |
| 图12 晶界与拉伸方向平行时FeMnCoCrNi、FeCuCoCrNi和Cu双晶的应力-应变曲线及原子结构 |
| Fig.12 Stress-strain curves (a1-a3), atomic structures of the [111] + [110] (b1-b3) and [123] + [110] (c1-c3) bicrystals when ε = 5%, ε = 20%, and ε = 100% of FeMnCoCrNi (a1-c1), FeCuCoCrNi (a2-c2), and Cu (a3-c3) bicrystals when the grain boundary is parallel to the tensile direction |
|