铁素体晶间变形协调与硬化行为模拟研究
|
|
徐永生, 张卫刚, 徐凌超, 但文蛟
|
Simulation of Deformation Coordination and Hardening Behavior in Ferrite-Ferrite Grain Boundary
|
|
XU Yongsheng, ZHANG Weigang, XU Lingchao, DAN Wenjiao
|
|
表3 <111>对称倾斜/扭转晶界双晶模型取向[27]
|
Table 3 Grain orientations in <111> axis symmetrically tilt/twist bicrystal models[27]
|
|
| Angle | Σ | Euler angle / (o) |
|---|
| (axis: <111>) | | Right grain | Left grain | | 0.00 | 1 | (0 0 0) | (0 0 0) | | 13.17 | 19 | (-136.9 5.37 133.1) | (46.9 5.37 -43.1) | | 21.79 | 7 | (-138.1 8.89 131.8) | (48.1 8.89 -41.8) | | 27.80 | 13 | (-139.0 11.34 131.0) | (49.0 11.34 -41.0) | | 32.20 | 13 | (-139.7 13.13 130.3) | (49.7 13.1 -40.3) | | 38.21 | 7 | (-140.5 15.6 129.5) | (50.5 15.6 -39.5) | | 46.82 | 19 | (-141.8 19.1 128.2) | (51.8 19.1 -38.2) | | 60.00 | 1 | (-143.8 24.4 126.2) | (53.8 24.4 -36.2) |
|
|
|