铁素体晶间变形协调与硬化行为模拟研究
|
|
徐永生, 张卫刚, 徐凌超, 但文蛟
|
Simulation of Deformation Coordination and Hardening Behavior in Ferrite-Ferrite Grain Boundary
|
|
XU Yongsheng, ZHANG Weigang, XU Lingchao, DAN Wenjiao
|
|
表2 <110>对称倾斜/扭转晶界双晶模型取向[27]
|
Table 2 Grain orientations in <110> axis symmetrically tilt/twist bicrystal models[27]
|
|
| Angle | Σ | Euler angle / (o) |
|---|
| (axis: <110>) | | Right grain | Left grain | | 0.00 | 1 | (0 0 0) | (0 0 0) | | 26.53 | 19 | (-135 13.26 135) | (45 13.26 -45) | | 31.59 | 27 | (-135 15.79 135) | (45 15.79 -45) | | 38.94 | 9 | (-135 19.47 135) | (45 19.47 -45) | | 50.48 | 11 | (-135 25.24 135) | (45 25.24 -45) | | 70.53 | 3 | (-135 35.26 135) | (45 35.26 -45) | | 109.47 | 3 | (-135 54.74 135) | (45 54.74 -45) | | 129.52 | 11 | (-135 64.76 135) | (45 64.76 -45) | | 141.06 | 9 | (-45 70.53 135) | (45 70.53 -45) | | 148.41 | 27 | (-135 74.21 135) | (45 74.21 -45) | | 180.00 | 1 | (-135 90 135) | (45 90 -45) |
|
|
|