铁素体晶间变形协调与硬化行为模拟研究
|
|
徐永生, 张卫刚, 徐凌超, 但文蛟
|
Simulation of Deformation Coordination and Hardening Behavior in Ferrite-Ferrite Grain Boundary
|
|
XU Yongsheng, ZHANG Weigang, XU Lingchao, DAN Wenjiao
|
|
表1 <100>对称倾斜/扭转晶界双晶模型晶粒取向[27]
|
Table 1 Grain orientations in <100> axis symmetrically tilt/twist bicrystal models[27]
|
|
| Angle | Σ | Euler angle / (o) |
|---|
| (axis: <100>) | | Right grain | Left grain | | 0.00 | 1 | (0 0 0) | (0 0 0) | | 16.26 | 25 | (180 8.13 180) | (0 8.13 0) | | 22.62 | 13 | (180 11.31 180) | (0 11.31 0) | | 28.07 | 17 | (180 14.04 180) | (0 14.04 0) | | 36.87 | 5 | (180 18.44 180) | (0 18.44 0) | | 53.13 | 5 | (180 26.57 180) | (0 26.57 0) | | 61.93 | 17 | (180 30.97 180) | (0 30.97 0) | | 67.38 | 13 | (180 33.69 180) | (0 33.69 0) | | 73.74 | 25 | (180 36.87 180) | (0 36.87 0) | | 90.00 | 1 | (180 45 180) | (0 45 0) |
|
|
|