铁素体晶间变形协调与硬化行为模拟研究 |
| 徐永生, 张卫刚, 徐凌超, 但文蛟 |
|
Simulation of Deformation Coordination and Hardening Behavior in Ferrite-Ferrite Grain Boundary |
| XU Yongsheng, ZHANG Weigang, XU Lingchao, DAN Wenjiao |
| 图3 不同应力状态下晶界区变形及其控制因素随倾转角度演化曲线 |
| Fig.3 Grain boundary strain ratios (a1-c1), resolve shear stress factors (a2-c2), and slip transfer factors m (a3-c3) and m* (a4-c4) curves with tilt angle (NO. represents the number of participants in the average after sorting the corresponding parameters from largest to smallest) (a1-a4) shear condition (b1-b4) uniaxial tension condition (c1-c4) plane strain condition |
|