结构功能一体化高锰减振钢研究发展概况 |
| 陈礼清, 李兴, 赵阳, 王帅, 冯阳 |
|
Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function |
| CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang |
| 图7 不同温度下Fe-17Mn-0.3Si减振钢的工程应力-应变和lnθ-lnσ曲线[ |
| Fig.7 Engineering stress-strain (θ-σ) (a) and lnθ-lnσ (b) curves of Fe-17Mn-0.3Si damping steel at different temperatures[ |
|