结构功能一体化高锰减振钢研究发展概况 |
| 陈礼清, 李兴, 赵阳, 王帅, 冯阳 |
|
Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function |
| CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang |
| 图6 Fe-15Mn、Fe-17Mn、Fe-19Mn和Fe-17Mn-0.3Si减振钢的工程应力-应变曲线和冲击功 |
| Fig.6 Engineering stress-strain curves (a) and impact energies (b) of Fe-15Mn, Fe-17Mn, Fe-19Mn, and Fe-17Mn-0.3Si damping steels |
|