结构功能一体化高锰减振钢研究发展概况
陈礼清, 李兴, 赵阳, 王帅, 冯阳

Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function
CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang
图4 Fe-15Mn和Fe-17Mn减振钢中观察到的变形诱导ε→γ相变[19]
Fig.4 Deformation-induced ε→γ transformation in Fe-15Mn and Fe-17Mn damping steels[19]
(a) austenitic orientation imaging map (OIM) in 5% deformed Fe-15Mn damping steel (Inset shows the standard inverse pole figure of austenite)
(b) EBSD phase map in 5% deformed Fe-15Mn damping steel (Red region denotes austenite, yellow region denotes ε-martensite, green region denotes α'-martensite. TD—transverse direction, RD—rolling direction)
(c) TEM image of 5% deformed Fe-17Mn damping steel (Inset shows the SAED pattern of γ phase)