基于中子与同步辐射技术的工程材料/部件多尺度残余应力评价 |
| 李时磊, 李阳, 王友康, 王胜杰, 何伦华, 孙光爱, 肖体乔, 王沿东 |
|
Multiscale Residual Stress Evaluation of Engineering Materials/Components Based on Neutron and Synchrotron Radiation Technology |
| LI Shilei, LI Yang, WANG Youkang, WANG Shengjie, HE Lunhua, SUN Guang'ai, XIAO Tiqiao, WANG Yandong |
| 图6 同步辐射高能X射线衍射技术测量梯度残余应力的原理及结果 |
| Fig.6 Schematic of the residual stress gradient measurement by HE-XRD (a), the acquisition of stress-free lattice spacing(d 0, indicated by red arrows) of (0002) crystal plane for the shot-peened zirconium alloy (b), and the distribution of residual stress along the depth direction in the shot-peened zirconium alloy (c) |
|