Cr2AlC涂层相结构演变对力学性能的影响
袁江淮, 王振玉, 马冠水, 周广学, 程晓英, 汪爱英

Effect of Phase-Structure Evolution on Mechanical Properties of Cr2AlC Coating
YUAN Jianghuai, WANG Zhenyu, MA Guanshui, ZHOU Guangxue, CHENG Xiaoying, WANG Aiying
表3 S1~S4样品硬度(H)、模量(E)、H / E和H 3 / E 2
Table 3 Hardness (H), elastic modulus (E), H / E, and H 3 / E 2 of samples S1-S4
SampleH / GPaE / GPaH / E(H 3 / E 2) / GPa
S112.39313.430.0400.020
S213.53330.740.0420.024
S311.12286.400.0390.017
S414.46345.170.0420.026