Cr2AlC涂层相结构演变对力学性能的影响 |
| 袁江淮, 王振玉, 马冠水, 周广学, 程晓英, 汪爱英 |
|
Effect of Phase-Structure Evolution on Mechanical Properties of Cr2AlC Coating |
| YUAN Jianghuai, WANG Zhenyu, MA Guanshui, ZHOU Guangxue, CHENG Xiaoying, WANG Aiying |
| 图6 S1~S4样品的Vickers压痕形貌 |
| Fig.6 Vickers indentation morphologies of samples S1 (a), S2 (b), S3 (c), and S4 (d) |
|