Cr2AlC涂层相结构演变对力学性能的影响 |
| 袁江淮, 王振玉, 马冠水, 周广学, 程晓英, 汪爱英 |
|
Effect of Phase-Structure Evolution on Mechanical Properties of Cr2AlC Coating |
| YUAN Jianghuai, WANG Zhenyu, MA Guanshui, ZHOU Guangxue, CHENG Xiaoying, WANG Aiying |
| 图2 Cr2AlC涂层及其在不同温度下退火2 h后的XRD谱 |
| Fig.2 XRD spectra of the Cr2AlC coatings before and after annealing at different temperatures for 2 h |
|