不同离子对TC4钛合金电化学腐蚀行为的协同作用机制 |
| 赵平平, 宋影伟, 董凯辉, 韩恩厚 |
|
Synergistic Effect Mechanism of Different Ions on the Electrochemical Corrosion Behavior of TC4 Titanium Alloy |
| ZHAO Pingping, SONG Yingwei, DONG Kaihui, HAN En-Hou |
| 图8 不同离子对钛合金极化曲线影响示意图 |
| Fig.8 Sketch maps of the effect of different ions on the polarazation curves of Ti alloy (a) F- (b) H+ + F- (c) H+ + F-+ Fe3+ |
|