9%Cr合金钢在含Cl-环境中的初期腐蚀行为及局部腐蚀起源 |
陈润农, 李昭东, 曹燕光, 张启富, 李晓刚 |
Initial Corrosion Behavior and Local Corrosion Origin of 9%Cr Alloy Steel in Cl-Containing Environment |
CHEN Runnong, LI Zhaodong, CAO Yanguang, ZHANG Qifu, LI Xiaogang |
图13 2种典型复合夹杂物在2%NaCl溶液中浸泡不同时间后的腐蚀形貌 |
Fig.13 Corrosion morphologies of MnS-rich (a1-a3) and MnS-poor (b1-b3) composite inclusions immersed in 2%NaCl solution for 5 min (a1, b1), 50 min (a2, b2), and 300 min (a3, b3) |
![]() |