9%Cr合金钢在含Cl-环境中的初期腐蚀行为及局部腐蚀起源 |
| 陈润农, 李昭东, 曹燕光, 张启富, 李晓刚 |
|
Initial Corrosion Behavior and Local Corrosion Origin of 9%Cr Alloy Steel in Cl-Containing Environment |
| CHEN Runnong, LI Zhaodong, CAO Yanguang, ZHANG Qifu, LI Xiaogang |
| 图3 9Cr钢腐蚀不同时间后的表面宏观和微观腐蚀形貌 |
| Fig.3 Macro (a1-a4) and micro (b1-b4) surface corrosion morphologies of 9Cr steels corroded for different time and the high-resolution SEM images (c1-c4) corresponding to the square areas in Figs.3b1-b4 (a1-c1) 72 h (a2-c2) 168 h (a3-c3) 264 h (a4-c4) 360 h |
|