Fe22Cr5Al3Mo-xY合金在模拟LOCA下的高温蒸汽氧化行为 |
|||||||||
| 孙蓉蓉, 姚美意, 王皓瑜, 张文怀, 胡丽娟, 仇云龙, 林晓冬, 谢耀平, 杨健, 董建新, 成国光 | |||||||||
|
High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition |
|||||||||
| SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang | |||||||||
| 表2 0Y和0.15Y合金在1000和1200℃高温蒸汽条件下恒温2 h的抛物线速率常数 (mg2·dm-4·s-1) |
|||||||||
| Table 2 Parabolic rate constants of 0Y and 0.15Y alloys oxidized in 1000 and 1200oC steam for 2 h |
|||||||||
|
|||||||||