Fe22Cr5Al3Mo-xY合金在模拟LOCA下的高温蒸汽氧化行为 |
| 孙蓉蓉, 姚美意, 王皓瑜, 张文怀, 胡丽娟, 仇云龙, 林晓冬, 谢耀平, 杨健, 董建新, 成国光 |
|
High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition |
| SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang |
| 图1 0Y和0.15Y合金的XRD谱 |
| Fig.1 XRD spectra of 0Y and 0.15Y alloys |
|