Cr添加对孪生诱发塑性钢腐蚀行为的影响 |
| 司永礼, 薛金涛, 王幸福, 梁驹华, 史子木, 韩福生 |
|
Effect of Cr Addition on the Corrosion Behavior of Twinning-Induced Plasticity Steel |
| SI Yongli, XUE Jintao, WANG Xingfu, LIANG Juhua, SHI Zimu, HAN Fusheng |
| 图12 基于XPS结果的样品表面膜的阳离子分数 |
| Fig.12 Cationic fractions in surface film of samples based on the XPS results |
|