Cr添加对孪生诱发塑性钢腐蚀行为的影响 |
| 司永礼, 薛金涛, 王幸福, 梁驹华, 史子木, 韩福生 |
|
Effect of Cr Addition on the Corrosion Behavior of Twinning-Induced Plasticity Steel |
| SI Yongli, XUE Jintao, WANG Xingfu, LIANG Juhua, SHI Zimu, HAN Fusheng |
| 图2 12Cr样品显微组织的OM像 |
| Fig.2 OM image of 12Cr sample |
|