EH36钢在不同粒径沙砾冲击下的冲刷腐蚀耦合损伤行为 |
| 张奇亮, 王玉超, 李光达, 李先军, 黄一, 徐云泽 |
|
Erosion-Corrosion Performance of EH36 Steel Under Sand Impacts of Different Particle Sizes |
| ZHANG Qiliang, WANG Yuchao, LI Guangda, LI Xianjun, HUANG Yi, XU Yunze |
| 图9 不同粒径沙砾冲击下碳钢的腐蚀分量、磨损分量、磨损加速腐蚀分量和腐蚀加速磨损分量 |
| Fig.9 Average steel losses induced by corrosion, erosion, erosion enhanced corrosion, and corrosion enhanced erosion under sand particle impacts of different sizes ( |
|