EH36钢在不同粒径沙砾冲击下的冲刷腐蚀耦合损伤行为 |
| 张奇亮, 王玉超, 李光达, 李先军, 黄一, 徐云泽 |
|
Erosion-Corrosion Performance of EH36 Steel Under Sand Impacts of Different Particle Sizes |
| ZHANG Qiliang, WANG Yuchao, LI Guangda, LI Xianjun, HUANG Yi, XU Yunze |
| 图8 3种不同粒径沙砾冲击下碳钢的纯磨损损伤形貌 |
| Fig.8 Photos, 3D profiles, and SEM images of the coupon electrodes after pure erosion of different size sand particles (Ra—roughness) (a) 100 μm (b) 430 μm (c) 850 μm |
|