低碳钢Q235、管线钢L415和压力容器钢16MnNi在湛江高湿高辐照海洋工业大气环境下的初期腐蚀行为 |
||||||||||||
| 李小涵, 曹公望, 郭明晓, 彭云超, 马凯军, 王振尧 | ||||||||||||
|
Initial Corrosion Behavior of Carbon Steel Q235, Pipeline Steel L415, and Pressure Vessel Steel 16MnNi Under High Humidity and High Irradiation Coastal-Industrial Atmosphere in Zhanjiang |
||||||||||||
| LI Xiaohan, CAO Gongwang, GUO Mingxiao, PENG Yunchao, MA Kaijun, WANG Zhenyao | ||||||||||||
| 表3 Q235、L415和16MnNi钢的腐蚀电位(Ecorr)和腐蚀电流密度(icorr) |
||||||||||||
| Table 3 Corrosion potential (Ecorr) and corrosion current density (icorr) of Q235, L415, and 16MnNi steels |
||||||||||||
|
||||||||||||