GH4169高温合金热机械疲劳循环损伤机理及数值模拟 |
| 张禄, 余志伟, 张磊成, 江荣, 宋迎东 |
|
Thermo-Mechanical Fatigue Cycle Damage Mechanism and Numerical Simulation of GH4169 Superalloy |
| ZHANG Lu, YU Zhiwei, ZHANG Leicheng, JIANG Rong, SONG Yingdong |
| 图8 GH4169高温合金不同加载条件下耗散能密度和TMF寿命 |
| Fig.8 GH4169 superalloy dissipative energy densities and TMF lives under different loading conditions |
|