GH4169高温合金热机械疲劳循环损伤机理及数值模拟 |
| 张禄, 余志伟, 张磊成, 江荣, 宋迎东 |
|
Thermo-Mechanical Fatigue Cycle Damage Mechanism and Numerical Simulation of GH4169 Superalloy |
| ZHANG Lu, YU Zhiwei, ZHANG Leicheng, JIANG Rong, SONG Yingdong |
| 图6 GH4169高温合金TMF寿命与低周疲劳(LCF)寿命[ |
| Fig.6 Comparisons of GH4169 superalloy TMF lives and isothermal low cycle fatigue (LCF) lives[ |
|