初始晶粒尺寸和强化相对GH4096高温合金热变形行为和再结晶的影响 |
||||||||||||||||||||
| 李福林, 付锐, 白云瑞, 孟令超, 谭海兵, 钟燕, 田伟, 杜金辉, 田志凌 | ||||||||||||||||||||
|
Effects of Initial Grain Size and Strengthening Phase on Thermal Deformation and Recrystallization Behavior of GH4096 Superalloy |
||||||||||||||||||||
| LI Fulin, FU Rui, BAI Yunrui, MENG Lingchao, TAN Haibing, ZHONG Yan, TIAN Wei, DU Jinhui, TIAN Zhiling | ||||||||||||||||||||
| 表2 不同初始组织试样(d1~d4)的平均α值、应力指数n和热变形激活能Q |
||||||||||||||||||||
| Table 2 Average ɑ values, stress index n and thermal deformation activation energies Q of samples d1-d4 |
||||||||||||||||||||
|
||||||||||||||||||||