初始晶粒尺寸和强化相对GH4096高温合金热变形行为和再结晶的影响 |
| 李福林, 付锐, 白云瑞, 孟令超, 谭海兵, 钟燕, 田伟, 杜金辉, 田志凌 |
|
Effects of Initial Grain Size and Strengthening Phase on Thermal Deformation and Recrystallization Behavior of GH4096 Superalloy |
| LI Fulin, FU Rui, BAI Yunrui, MENG Lingchao, TAN Haibing, ZHONG Yan, TIAN Wei, DU Jinhui, TIAN Zhiling |
| 图17 铸态试样(c1和c2)经过1060℃、0.1 s-1热压缩(50%)后显微组织的TEM像 |
| Fig.17 TEM images of as-cast c1 and c2 samples after hot compression 50% at 1060oC, 0.1 s-1 (a, b) c1 sample, grain boundary absorbing lots of dislocation lines (c, d) c2 sample, showing γ' stimulated DRX nucleation |
|