初始晶粒尺寸和强化相对GH4096高温合金热变形行为和再结晶的影响 |
| 李福林, 付锐, 白云瑞, 孟令超, 谭海兵, 钟燕, 田伟, 杜金辉, 田志凌 |
|
Effects of Initial Grain Size and Strengthening Phase on Thermal Deformation and Recrystallization Behavior of GH4096 Superalloy |
| LI Fulin, FU Rui, BAI Yunrui, MENG Lingchao, TAN Haibing, ZHONG Yan, TIAN Wei, DU Jinhui, TIAN Zhiling |
| 图13 粗晶d2试样在1100℃、0.1 s-1,工程应变为30%和50%时热压缩后显微组织的TEM像 |
| Fig.13 TEM images of coarsen grained d2 samples after hot compression at 1100oC, 0.1 s-1 (a) 30% engineering strain (b) 50% engineering strain |
|