初始晶粒尺寸和强化相对GH4096高温合金热变形行为和再结晶的影响 |
| 李福林, 付锐, 白云瑞, 孟令超, 谭海兵, 钟燕, 田伟, 杜金辉, 田志凌 |
|
Effects of Initial Grain Size and Strengthening Phase on Thermal Deformation and Recrystallization Behavior of GH4096 Superalloy |
| LI Fulin, FU Rui, BAI Yunrui, MENG Lingchao, TAN Haibing, ZHONG Yan, TIAN Wei, DU Jinhui, TIAN Zhiling |
| 图8 不同初始晶粒尺寸的试样(d1~d4)在应变速率为0.1 s-1和工程应变为50%时不同温度下热压缩后的金相组织 |
| Fig.8 OM images of samples d1 (a, b), d2 (c, d), d3 (e, f), and d4 (g, h) under hot compression at different temperatures, the strain rate of 0.1 s-1, and the engineering strain of 50% (a, c, e, g) 1120oC (b, d, f, h) 1080oC |
|