初始晶粒尺寸和强化相对GH4096高温合金热变形行为和再结晶的影响 |
| 李福林, 付锐, 白云瑞, 孟令超, 谭海兵, 钟燕, 田伟, 杜金辉, 田志凌 |
|
Effects of Initial Grain Size and Strengthening Phase on Thermal Deformation and Recrystallization Behavior of GH4096 Superalloy |
| LI Fulin, FU Rui, BAI Yunrui, MENG Lingchao, TAN Haibing, ZHONG Yan, TIAN Wei, DU Jinhui, TIAN Zhiling |
| 图5 c1和c2试样热压缩过程的动态再结晶临界应变(应变速率为0.1 s-1) |
| Fig.5 Critical strain of dynamic recrystallization (DRX) of samples c1 and c2 in as-cast state at the strain rate of 0.1 s-1 |
|