初始晶粒尺寸和强化相对GH4096高温合金热变形行为和再结晶的影响 |
| 李福林, 付锐, 白云瑞, 孟令超, 谭海兵, 钟燕, 田伟, 杜金辉, 田志凌 |
|
Effects of Initial Grain Size and Strengthening Phase on Thermal Deformation and Recrystallization Behavior of GH4096 Superalloy |
| LI Fulin, FU Rui, BAI Yunrui, MENG Lingchao, TAN Haibing, ZHONG Yan, TIAN Wei, DU Jinhui, TIAN Zhiling |
| 图3 不同初始组织试样(d1~d4)在应变速率为0.1 s-1和不同温度下热压缩的真应力-真应变曲线及峰值流变应力曲线 |
| Fig.3 True stress-strain curves (a-d) and peak stress curves (e) of samples d1-d4 under thermal compression at the strain rate of 0.1 s-1 and different temperatures (a) 1060oC (b) 1080oC (c) 1100oC (d) 1120oC (e) comparison of peak stress |
|