基于高通量场发射扫描电镜建立的高温合金 γ' 相定量统计表征方法 |
| 卢毓华, 王海舟, 李冬玲, 付锐, 李福林, 石慧 |
|
A Quantitative and Statistical Method of γ' Precipitates in Superalloy Based on the High-Throughput Field Emission Scanning Eelectron Microscope |
| LU Yuhua, WANG Haizhou, LI Dongling, FU Rui, LI Fulin, SHI Hui |
| 图10 Recipe-2和Recipe-2 +人工修正2种方式对CR-4样品169张57000倍图像中二次和三次γ'相的数量、平均尺寸、尺寸中位值的统计结果对比 |
| Fig.10 Comparisons of total amount (a), average diameter (b), and the median diameter (c) of secondary and tertiary γ' precipitates in 169 images with magnification of 57000 in samples CR-4 between Recipe-2 and Recipe-2 & manual, two ways to recognized γ' precipitates |
|