基于高通量场发射扫描电镜建立的高温合金 γ' 相定量统计表征方法 |
| 卢毓华, 王海舟, 李冬玲, 付锐, 李福林, 石慧 |
|
A Quantitative and Statistical Method of γ' Precipitates in Superalloy Based on the High-Throughput Field Emission Scanning Eelectron Microscope |
| LU Yuhua, WANG Haizhou, LI Dongling, FU Rui, LI Fulin, SHI Hui |
| 图7 CR-1~CR-5样品57000倍图像中二次和三次γ'相数量随图像张数的变化 |
| Fig.7 Tendencies of the amount of secondary (a) and tertiary (b) γ' precipitates with magnification of 57000 in samples CR-1-CR-5 varied with the amount of image |
|