基于高通量场发射扫描电镜建立的高温合金 γ' 相定量统计表征方法 |
| 卢毓华, 王海舟, 李冬玲, 付锐, 李福林, 石慧 |
|
A Quantitative and Statistical Method of γ' Precipitates in Superalloy Based on the High-Throughput Field Emission Scanning Eelectron Microscope |
| LU Yuhua, WANG Haizhou, LI Dongling, FU Rui, LI Fulin, SHI Hui |
| 图3 对57000倍SEM像中一次、二次和三次γ'相建立识别Recipe-2的几个主要步骤 |
| Fig.3 Main procedures on building the Recipe-2 for characterizing primary, secondary, and tertiary γ' precipitates in SEM images with magnification of 57000 |
|