弹性拉应力下Q235碳钢在5%NaCl盐雾中的成锈行为及其机理 |
| 李谦, 刘凯, 赵天亮 |
|
Rust Formation Behavior and Mechanism of Q235 Carbon Steel in 5%NaCl Salt Spray Under Elastic Tensile Stress |
| LI Qian, LIU Kai, ZHAO Tianliang |
| 图11 加载方式A和B下等效电路中电荷转移电阻(Rct)、锈层电阻(Rrust)与电容弥散系数(nrust)、扩散阻抗(W)随弹性拉应力水平的变化趋势 |
| Fig.11 Variations of Rct, Rrust (a) and nrust, W (b) in the equivalent electric circuit with elastic tensile stress levels under loading modes A and B |
|