弹性拉应力下Q235碳钢在5%NaCl盐雾中的成锈行为及其机理 |
| 李谦, 刘凯, 赵天亮 |
|
Rust Formation Behavior and Mechanism of Q235 Carbon Steel in 5%NaCl Salt Spray Under Elastic Tensile Stress |
| LI Qian, LIU Kai, ZHAO Tianliang |
| 图7 Q235碳钢在5%NaCl盐雾中暴露15 d后锈层的单位面积质量和密度随钢基体所受弹性拉应力水平的变化 |
| Fig.7 Variations of mass per unit area and density of the rust layer with the elastic tensile stress level for Q235 carbon steel after exposed in 5%NaCl salt spray for 15 d |
|