弹性拉应力下Q235碳钢在5%NaCl盐雾中的成锈行为及其机理 |
| 李谦, 刘凯, 赵天亮 |
|
Rust Formation Behavior and Mechanism of Q235 Carbon Steel in 5%NaCl Salt Spray Under Elastic Tensile Stress |
| LI Qian, LIU Kai, ZHAO Tianliang |
| 图6 不同弹性拉应力水平下Q235碳钢在5%NaCl盐雾中暴露15 d后锈层的XRD谱和物相组成 |
| Fig.6 XRD spectra (a) and phase compositions (b) in the rust layer of Q235 carbon steel under various elastic tensile stress levels after exposed in 5%NaCl salt spray for 15 d |
|