冷轧中碳梯度马氏体钢的组织与力学性能 |
| 王周头, 袁清, 张庆枭, 刘升, 徐光 |
|
Microstructure and Mechanical Properties of a Cold Rolled Gradient Medium-Carbon Martensitic Steel |
| WANG Zhoutou, YUAN Qing, ZHANG Qingxiao, LIU Sheng, XU Guang |
| 图6 轧制后试样总体形貌图 |
| Fig.6 Morphologies of the cold rolled specimens of homogeneous martensite (sample 1) and compositionally gradient martensite (sample 2) (a) and enlarged view of homogeneous martensite in sample 1 (b) |
|