新型耐热合金SP2215组织与性能的关联性 |
| 梁凯, 姚志浩, 谢锡善, 姚凯俊, 董建新 |
|
Correlation Between Microstructure and Properties of New Heat-Resistant Alloy SP2215 |
| LIANG Kai, YAO Zhihao, XIE Xishan, YAO Kaijun, DONG Jianxin |
| 图11 650℃时效500 h的MX相、6000 h的NbCrN相,及700℃时效6000 h的NbCrN相的TEM像 |
| Fig.11 TEM images of MX precipitates after aging at 650oC for 500 h (a), and NbCrN precipitates after aging at 650oC (b) and 700oC (c) for 6000 h |
|