新型耐热合金SP2215组织与性能的关联性 |
| 梁凯, 姚志浩, 谢锡善, 姚凯俊, 董建新 |
|
Correlation Between Microstructure and Properties of New Heat-Resistant Alloy SP2215 |
| LIANG Kai, YAO Zhihao, XIE Xishan, YAO Kaijun, DONG Jianxin |
| 图8 SP2215耐热合金在不同时效温度下lnln[1 / (1 - f)]与lnt的关系曲线 |
| Fig.8 Fitting curves of lnln[1 / (1 - f)] and lnt of SP2215 heat-resistant alloy at different aging temperatures (f—conversion rate of M23C6 phase) |
|