新型耐热合金SP2215组织与性能的关联性 |
| 梁凯, 姚志浩, 谢锡善, 姚凯俊, 董建新 |
|
Correlation Between Microstructure and Properties of New Heat-Resistant Alloy SP2215 |
| LIANG Kai, YAO Zhihao, XIE Xishan, YAO Kaijun, DONG Jianxin |
| 图7 M23C6含量随时效时间的变化曲线 |
| Fig.7 Volume fractions of M23C6 as a function of aging time at different aging temperatures |
|