高合金化GH4151合金复杂析出相演变行为 |
| 王法, 江河, 董建新 |
|
Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy |
| WANG Fa, JIANG He, DONG Jianxin |
| 图4 基于关键温度区间确立的热处理条件下GH4151合金显微组织的SEM像 |