Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy |
| WANG Fa, JIANG He, DONG Jianxin |
| 图3 GH4151合金不同温度保温10 min后水冷组织形貌的SEM像 |
| Fig.3 SEM images of GH4151 superalloy after heat treated at 1150oC (a, b), 1160oC (c, d), 1170oC (e), 1180oC (f), and 1190oC (g) for 10 min and then water quenching |
|