高合金化GH4151合金复杂析出相演变行为 |
| 王法, 江河, 董建新 |
|
Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy |
| WANG Fa, JIANG He, DONG Jianxin |
| 图1 GH4151合金凝固过程的元素分布及凝固路径的热力学计算结果 |
| Fig.1 Thermodynamic calculation results of element distribution behavior during solidification (a) and solidification process (b) of GH4151 superalloy |
|