低密度Ti2AlNb基合金热轧板微观组织的热稳定性 |
| 冯艾寒, 陈强, 王剑, 王皞, 曲寿江, 陈道伦 |
|
Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate |
| FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun |
| 图4 Ti2AlNb基合金热轧板在不同温度保温12 h前后的XRD谱 |
| Fig.4 XRD spectra of hot rolled Ti2AlNb-based alloys plate before (a) and after heat treatment at 600oC (b), 800oC (c), 850oC (d), 900oC (e), 950oC (f), 1000oC (g), 1050oC (h), and 1100oC (i) for 12 h and then water quenching (Insets in Figs.4c-e show the magnified spectra) |
|