低密度Ti2AlNb基合金热轧板微观组织的热稳定性 |
| 冯艾寒, 陈强, 王剑, 王皞, 曲寿江, 陈道伦 |
|
Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate |
| FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun |
| 图3 Ti2AlNb基合金热轧板在不同温度保温12 h水淬后的SEM像 |
| Fig.3 SEM images of hot rolled Ti2AlNb-based alloy plate after heat treatment at 600oC (a), 800oC (b), 900oC (c), 950oC (d), 1000oC (e), and 1100oC (f) for 12 h and then water quenching |
|