电弧增材制造2024铝合金的微观组织与力学性能 |
| 吴东江, 刘德华, 张子傲, 张逸伦, 牛方勇, 马广义 |
|
Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing |
| WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi |
| 图7 2024铝合金WAAM成形试样面扫描元素分布 |
| Fig.7 Element mapping of WAAM 2024 aluminum alloy deposited specimen |
|