微电子互连用锡基合金及复合钎料热-机械可靠性研究进展
郭福, 杜逸晖, 籍晓亮, 王乙舒

Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection
GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu
图5 Ag纳米颗粒包覆的多壁碳纳米管(MWCNTs)的TEM像[80]
Fig.5 TEM image of multi-walled carbon nanotubes (MWCNTs) coated by Ag nanoparticles[80]