高熵合金的低温塑性变形机制及强韧化研究进展 |
| 刘俊鹏, 陈浩, 张弛, 杨志刚, 张勇, 戴兰宏 |
|
Progress of Cryogenic Deformation and Strengthening-Toughening Mechanisms of High-Entropy Alloys |
| LIU Junpeng, CHEN Hao, ZHANG Chi, YANG Zhigang, ZHANG Yong, DAI Lanhong |
| 图13 热拉拔CoCrNi丝材的室温及低温力学性能[ |
| Fig.13 Tensile properties of hot-drawing CoCrNi wire at room and cryogenic temperatures[ |
|